Pure Nickel Capillary Tube
Product Details:
|
|
Place of Origin: | CHINA |
---|---|
Brand Name: | JINXING |
Certification: | ISO 9001 |
Model Number: | Kovar Tube |
Payment & Shipping Terms:
|
|
Minimum Order Quantity: | 50KGS |
Price: | 15~50USD/kg |
Packaging Details: | Plywood Case |
Delivery Time: | 25 work days |
Payment Terms: | L/C, D/A, D/P, T/T, Western Union |
Supply Ability: | 100000kgs/M |
Detail Information |
|||
Material: | Kovar Alloy K UNS K94610 | Surface: | Pickled , Polished |
---|---|---|---|
Standard: | ASTM F15 | Heat Treatment: | Solution Annealed |
Size: | Customized | Application: | Glass Sealing |
Density: | 8.36g/cm3 | Melting Point: | 1450C |
Highlight: | ni based superalloys,ni based alloys |
Product Description
Kovar alloy tube , Alloy K / UNS K94610 / ASTM F15
Alloy K / K94610 / ASTM F15 Also known as Kovar*** and Nilo K**, this alloy contains 29% nickel with a 17% cobalt addition. Its composition is tightly controlled within narrow limits to ensure precise and universal thermal expansion and mechanical characteristics. This helps the material provide high integrity glass-to-metal and ceramic-to-metal seals in applications requiring reliability and resistance to thermal shock. Alloy K is often used for the manufacture of hermetic seals with both the harder Pyrex or borosilicate glasses and alumina-type ceramic materials. It finds extensive application in the production of transistors and diodes for lids and closures in a variety of hybrid electronic circuit packages and also in the manufacture of microwave tubes.
Main Application:
Matching sealing in electric vacuum industry and hard glass
Material :
Russia | USA | England | Japan | Franch | Germany |
29HK | kovar | Nilo K | KV-1 | Dilvar P0 | Vacon 12 |
29HK-B | Rodar Techallony Glasseal 29-17 |
Teleaseal | KV-2 KV-3 |
Dilver P1 | Silvar |
Content Composition %
C | P | S | Mn | Si | Cu | Cr | Mo | Ni | Co | Fe |
Less than | ||||||||||
0.03 | 0.02 | 0.02 | 0.5 | 0.3 | 0.2 | 0.2 | 0.2 | 28.5-29.5 | 16.8-17.8 | Rest |
Physical properties
Density | g/cm3 | 8.25 |
Curie Point | ℃ | 430 |
Resistivity | μ· m | 0.48 |
Tensile strength Mpa | Cold state | |
Annealing | 520 | |
Yield strength Mpa | Cold state | |
Annealing | 330 | |
Elongation % | Cold state | |
annealing | 30 |
The linear expansion coefficient of the kovar alloy is similar to that of borosilicate glass at 20-450 ℃, the Curie point is higher, and the alloy has good low temperature structure stability. The oxide film of the alloy is compact and can be well infiltrated by glass. It does not interact with mercury and is suitable for use in instruments containing mercury discharge. It is the main sealing structure material of electric vacuum device.
Enter Your Message